Case-hardened ball
Physical Property | |
---|---|
Corrosion Resistant | No |
Wear Resistant | Good |
Magnetism | Yes |
Technical Data | |
---|---|
Hardness | HRC 55 – 65 |
Density | 7.82g/m3 |
Young’s Modulus | 200GPa |
Tensile Strength | 300-400MPa |
Chemical Composition | |||||
---|---|---|---|---|---|
Type | %C | %Si | %Mn | %P | %S |
1010 | 0.08 – 0.13 | 0.10 – 0.35 | 0.30 – 0.60 | 0.040 Max | 0.050 Max |
1015 | 0.12 – 0.18 | 0.10 – 0.35 | 0.30 – 0.60 | 0.040 Max | 0.050 Max |
International Standard | |||||||
---|---|---|---|---|---|---|---|
USA | CHN | GER | FRA | UK | ITA | RUS | JPN |
1010 | 10 | 1.1121 | CC10 | 040A10 | C10 | 10 | S10C |
1015 | 15 | 1.1141 | XC12 | 080M15 | C15 | 15 | S15C |
Cash Depth | |||
---|---|---|---|
Ball Diameter | Min. Case Depth | Ball Diameter | Min. Case Depth |
2.0-3.0mm | 0.5mm | 9.5-11.0mm | 1.4mm |
3.1-4.5mm | 0.6mm | 11.1-12.5mm | 1.7mm |
4.6-5.5mm | 0.8mm | 12.6-14.0mm | 1.8mm |
5.6-6.5mm | 0.9mm | 14.1-19.0mm | 1.9mm |
6.6-9.5mm | 1.1mm | 19.1-38.0mm | 2.0mm |
Get in touch with us today for any service. (*) Indicates required fields.